T1 - Avoiding electrochemical indentations
T2 - a CNT-cocooned LiCoO2 electrode with ultra-stable high-voltage cycling
AU - Zhu, Zhi
AU - Xu, Shuanglong
AU - Wang, Zhenjie
AU - Yan, Xiaohui
AU - Xu, Guiyin
AU - Huang, Yimeng
AU - Wu, Yuping
AU - Zhang, Yin
AU - Li, Ju
N1 - Publisher Copyright:
© 2024 The Royal Society of Chemistry.
PY - 2024/7/25
Y1 - 2024/7/25
N2 - Charging LiCoO2 (LCO) to above 4.5 V induces crystal cracking and seriously deteriorates the battery cycle life. Decreasing the range of the LCO misfit strain during deep de-lithiation is useful for preventing cracks, but this is not always achievable. Here, we demonstrate that the limited electrochemical contact area between electronically conductive carbon and the LCO crystal causes “electrochemical indentations” (ECIs) during charging and discharging. Particularly in fast charging, the high local ΔcLi gradient in LCO would cause a local volume of the surficial lattice to shrink while the rest of the crystal is still under stretching, and hence, drive the ECI to cause cracking. Increasing the electrochemical contact area would reduce the ECI and cracking risk. Therefore, we developed a free-standing CNT-LCO electrode in which all of the LCO particles were intimately wrapped with a dense CNT cocoon to establish a larger true electrical contact area. The simulations demonstrated that the radial ΔcLi and ECI decreased significantly in the cocooned LCO particles. The cocooned LCO electrode maintained good morphology and retained 94% of its energy density after 400 cycles when charged to 4.55 V. By removing the need for a current collector and binder, the volumetric energy density of the CNT-LCO cathode reached 3200 Wh L−1 (electrode).
AB - Charging LiCoO2 (LCO) to above 4.5 V induces crystal cracking and seriously deteriorates the battery cycle life. Decreasing the range of the LCO misfit strain during deep de-lithiation is useful for preventing cracks, but this is not always achievable. Here, we demonstrate that the limited electrochemical contact area between electronically conductive carbon and the LCO crystal causes “electrochemical indentations” (ECIs) during charging and discharging. Particularly in fast charging, the high local ΔcLi gradient in LCO would cause a local volume of the surficial lattice to shrink while the rest of the crystal is still under stretching, and hence, drive the ECI to cause cracking. Increasing the electrochemical contact area would reduce the ECI and cracking risk. Therefore, we developed a free-standing CNT-LCO electrode in which all of the LCO particles were intimately wrapped with a dense CNT cocoon to establish a larger true electrical contact area. The simulations demonstrated that the radial ΔcLi and ECI decreased significantly in the cocooned LCO particles. The cocooned LCO electrode maintained good morphology and retained 94% of its energy density after 400 cycles when charged to 4.55 V. By removing the need for a current collector and binder, the volumetric energy density of the CNT-LCO cathode reached 3200 Wh L−1 (electrode).
UR - http://www.scopus.com/inward/record.url?scp=85199694963&partnerID=8YFLogxK
U2 - 10.1039/d4ee00722k
DO - 10.1039/d4ee00722k
M3 - 文章
AN - SCOPUS:85199694963
SN - 1754-5692
VL - 17
SP - 6102
EP - 6112
JO - Energy and Environmental Science
JF - Energy and Environmental Science
IS - 16
ER -