Abstract
Microstructure and mechanical properties of as-cast and heat-treated Mg-12.3Zn-5.8Y-1.4Al (ZYA1261) alloy were investigated. The phase compositions of the as-cast alloy are α-Mg, Mg3YZn6 (I-phase), Mg3Y2Zn3 (W-phase), Mg12YZn (Z-phase), Mg24Y5, MgZn and a small quantity of Al-containing phase. The phase compositions change with various heat treatment conditions. The highest Vickers hardness is obtained in the alloy aged at 200 °C for 5 h, the transmission electron microscopy indicated that fine scale Z-phase precipitates in the matrix. The tensile properties of the as-cast and heat-treated alloys were reported.
Original language | English |
---|---|
Pages (from-to) | 55-60 |
Number of pages | 6 |
Journal | Materials Science and Engineering: A |
Volume | 485 |
Issue number | 1-2 |
DOIs | |
State | Published - 25 Jun 2008 |
Externally published | Yes |
Keywords
- Heat treatment
- Mechanical properties
- Mg-Zn-Y-Al alloy
- Microstructure