N2 - Sulfated zirconia catalysts are proposed for the reversible hydrolysis of ethyl lactate instead of liquid acids. Sulfated zirconia catalysts were prepared by precipitation-impregnation method. The zirconium hydroxide was produced from zirconium oxychloride by adding aqueous ammonia and then impregnated in sulfuric acid. The solid samples were obtained by filtration and evaporation of the mixtures, respectively. After the samples were calcined, the sulfated zirconia catalysts were prepared. The results showed that the catalyst prepared by evaporation has higher catalytic activity. The physicochemical characteristics of the sulfated zirconia catalysts were studied by thermal analysis, X-ray powder diffraction (XRD), temperature programmed desorption of ammonia (NH3-TPD) and N2 adsorption-desorption, respectively. By the precipitation-impregnation-evaporation method, the optimal sulfated zirconia catalyst of tetragonal phase was prepared under liquid-solid ratio of 5ml/g, 1 mol/L of H2SO4 and calcination at 650 °C for 3 h. The conversion of the ethyl lactate was 87.8% in 3 h at 85 °C with the catalyst loading 2 wt% and initial molar ratio of water to ethyl lactate 20: 1.
AB - Sulfated zirconia catalysts are proposed for the reversible hydrolysis of ethyl lactate instead of liquid acids. Sulfated zirconia catalysts were prepared by precipitation-impregnation method. The zirconium hydroxide was produced from zirconium oxychloride by adding aqueous ammonia and then impregnated in sulfuric acid. The solid samples were obtained by filtration and evaporation of the mixtures, respectively. After the samples were calcined, the sulfated zirconia catalysts were prepared. The results showed that the catalyst prepared by evaporation has higher catalytic activity. The physicochemical characteristics of the sulfated zirconia catalysts were studied by thermal analysis, X-ray powder diffraction (XRD), temperature programmed desorption of ammonia (NH3-TPD) and N2 adsorption-desorption, respectively. By the precipitation-impregnation-evaporation method, the optimal sulfated zirconia catalyst of tetragonal phase was prepared under liquid-solid ratio of 5ml/g, 1 mol/L of H2SO4 and calcination at 650 °C for 3 h. The conversion of the ethyl lactate was 87.8% in 3 h at 85 °C with the catalyst loading 2 wt% and initial molar ratio of water to ethyl lactate 20: 1.
KW - Catalyst, Precipitation-impregnation Method
KW - Ethyl Lactate
KW - Hydrolysis
KW - Sulfated Zirconia
UR - http://www.scopus.com/inward/record.url?scp=84878545152&partnerID=8YFLogxK
U2 - 10.1007/s11814-013-0036-5
DO - 10.1007/s11814-013-0036-5
M3 - 文章
AN - SCOPUS:84878545152
SN - 0256-1115
VL - 30
SP - 1222
EP - 1228