Abstract
In the present paper, difficulties in material data sampling and lifetime estimation are discussed. A local deformation measuring technique is proposed to determine the creep properties of the weld. A damage mechanics approach is introduced to study the damage development and creep rupture of HK-40 furnace tubes due to the presence of a weld. It has been illustrated that damage is prone to the weld in the later period of service life. Metallographical research also indicates that the weld may have a higher damage rank. It is thus concluded that the weldments may become the weak link in HK-40 furnace tubes.