N2 - This study investigated the sulfate resistance of Portland-dolomite cement (PDC) cured at different temperatures. Mortars of Portland cement (PC) and PDC with different dosages of dolomite, 10, 20, 30% by weight, were cured in water at 20 °C and 60 °C for 28 days before immersed in 50 g/L Na2SO4 solution at 20 °C. In addition to monitoring the length changes of mortars, MIP and XRD were performed to investigate microstructure and evolution of phase assemblages. Results show that PDC mortars cured at 20 °C give a poorer sulfate resistance than PC, and the higher the dosage of dolomite, the worse the sulfate resistance. On the contrary, when cured at 60 °C, PDC gives a much better sulfate resistance than PC, and the higher the dosage of dolomite, the better the sulfate resistance. The increases of critical pore size and porosity with the incorporation of dolomite lead to a poor sulfate resistance of PDC cured at 20 °C. However, for PDC cured at 60 °C, it is not the pore structure but the lack of available aluminate caused by the formation of hydrotalcite contributes to its sound sulfate resistance. The higher the dosage of dolomite from 10 to 30%, the larger amounts of hydrotalcite formation and the better the sulfate resistance. Hydrotalcite is stable in the presence of sulfate.
AB - This study investigated the sulfate resistance of Portland-dolomite cement (PDC) cured at different temperatures. Mortars of Portland cement (PC) and PDC with different dosages of dolomite, 10, 20, 30% by weight, were cured in water at 20 °C and 60 °C for 28 days before immersed in 50 g/L Na2SO4 solution at 20 °C. In addition to monitoring the length changes of mortars, MIP and XRD were performed to investigate microstructure and evolution of phase assemblages. Results show that PDC mortars cured at 20 °C give a poorer sulfate resistance than PC, and the higher the dosage of dolomite, the worse the sulfate resistance. On the contrary, when cured at 60 °C, PDC gives a much better sulfate resistance than PC, and the higher the dosage of dolomite, the better the sulfate resistance. The increases of critical pore size and porosity with the incorporation of dolomite lead to a poor sulfate resistance of PDC cured at 20 °C. However, for PDC cured at 60 °C, it is not the pore structure but the lack of available aluminate caused by the formation of hydrotalcite contributes to its sound sulfate resistance. The higher the dosage of dolomite from 10 to 30%, the larger amounts of hydrotalcite formation and the better the sulfate resistance. Hydrotalcite is stable in the presence of sulfate.
KW - Hydrotalcite
KW - Mechanism
KW - Portland-dolomite cement
KW - Sulfate attack
UR - http://www.scopus.com/inward/record.url?scp=85091719415&partnerID=8YFLogxK
U2 - 10.1617/s11527-020-01557-x
DO - 10.1617/s11527-020-01557-x
M3 - 文章
AN - SCOPUS:85091719415
SN - 1359-5997
VL - 53
JO - Materials and Structures/Materiaux et Constructions
JF - Materials and Structures/Materiaux et Constructions
IS - 5
M1 - 125
ER -