Atomic layer deposition of Al2O3 on porous polypropylene hollow fibers for enhanced membrane performances

Xiaojuan Jia, Zexian Low, He Chen, Sen Xiong, Yong Wang

科研成果: 期刊稿件文章同行评审

18 引用 (Scopus)

摘要

Porous polypropylene hollow fiber (PPHF) membranes are widely used in liquid purification. However, the hydrophobicity of polypropylene (PP) has limited its applications in water treatment. Herein, we demonstrate that, for the first time, atomic layer deposition (ALD) is an effective strategy to conveniently upgrade the filtration performances of PPHF membranes. The chemical and morphological changes of the deposited PPHF membranes are characterized by spectral, compositional, microscopic characterizations and protein adsorption measurements. Al2O3 is distributed along the cross section of the PP hollow fibers, with decreasing concentration from the outer surface to the inner surface. The pore size of the outer surface can be easily turned by altering the ALD cycles. Interestingly, the hollow fibers become much more ductile after deposition as their elongation at break is increased more than six times after deposition with 100 cycles. The deposited membranes show simultaneously enhanced water permeance and retention after deposition with moderate ALD cycle numbers. For instance, after 50 ALD cycles a 17% increase in water permeance and one-fold increase in BSA rejection are observed. Moreover, the PP membranes exhibit improved fouling-resistance after ALD deposition.

源语言英语
页(从-至)695-700
页数6
期刊Chinese Journal of Chemical Engineering
26
4
DOI
出版状态已出版 - 4月 2018

指纹

探究 'Atomic layer deposition of Al2O3 on porous polypropylene hollow fibers for enhanced membrane performances' 的科研主题。它们共同构成独一无二的指纹。

引用此