Development of a Ni-Ce0.8Zr0.2O2 catalyst for solid oxide fuel cells operating on ethanol through internal reforming

Mingming Liao, Wei Wang, Ran Ran, Zongping Shao

科研成果: 期刊稿件文章同行评审

47 引用 (Scopus)

摘要

Inexpensive 20 wt.% Ni-Ce0.8Zr0.2O2 catalysts are synthesized by a glycine nitrate process (GNP) and an impregnation process (IMP). The catalytic activity for ethanol steam reforming (ESR) at 400-650 °C, catalytic stability and carbon deposition properties are investigated. Ni-Ce0.8Zr0.2O2 (GNP) shows a higher catalytic performance than Ni-Ce0.8Zr0.2O 2 (IMP), especially at lower temperatures. It also presents a better coking resistance and a lower graphitization degree of the deposited carbon. The superior catalytic activity and coke resistance of Ni-Ce0.8Zr 0.2O2 (GNP) is attributed to the small particle size of the active metallic nickel phase and the strong interaction between the nickel and the Ce0.8Zr0.2O2 support, as evidenced by the XRD and H2-TPR. The Ni-Ce0.8Zr0.2O 2 (GNP) is further applied as an anode functional layer in solid oxide fuel cells operating on ethanol steam. The cell yields a peak power density of 536 mW cm-2 at 700 °C when operating on EtOH-H 2O gas mixtures, which is only slightly lower than that of hydrogen fuel, whereas the cell without the functional layer failed for short-term operations. Ni-Ce0.8Zr0.2O2 (GNP) is promising as an active and highly coking-resistant catalyst layer for solid-oxide fuel cells operating on ethanol steam fuel.

源语言英语
页(从-至)6177-6185
页数9
期刊Journal of Power Sources
196
15
DOI
出版状态已出版 - 1 8月 2011

指纹

探究 'Development of a Ni-Ce0.8Zr0.2O2 catalyst for solid oxide fuel cells operating on ethanol through internal reforming' 的科研主题。它们共同构成独一无二的指纹。

引用此