TY - JOUR
T1 - Effect of calcination temperature on oxidation state of cobalt in calcium cobaltite and relevant performance as intermediate-temperature solid oxide fuel cell cathodes
AU - Yu, Shancheng
AU - He, Shoucheng
AU - Chen, Han
AU - Guo, Lucun
N1 - Publisher Copyright:
© 2015 Elsevier B.V. All rights reserved.
PY - 2015/4/15
Y1 - 2015/4/15
N2 - (Graph Presented) Calcium cobaltite materials are synthesized by calcining the mixture of CaCO3 and Co3O4 with the Ca: Co ratio of 3:4. The reactivity of CaCO3 with Co3O4 is evaluated by thermogravimetric analysis (TGA), X-ray powder diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). Thermal expansion coefficient (TEC), electrical conductivity and electrochemical performance as intermediate-temperature solid oxide fuel cells (IT-SOFCs) cathode of as-prepared materials are characterized. The experiment results show that simultaneous decomposition of CaCO3 with calcium cobaltite formation occurs at 650-900°C. The average valence for Co ions of calcium cobaltite increases with temperature in the range of 750-900°C, involved in the formation of the compounds Ca3Co4O9 and Ca9Co12O28 at 800 and 900°C, respectively. The performance of calcium cobaltite cathodes applied in IT-SOFCs is significantly effected by the oxidation state of cobalt ions. As a result, Ca9Co12O28 cathode has a lower area specific resistance (e.g. 41.8% lower at 800°C) and higher peak power density (e.g. 45.0% higher at 800° C) than the cathode of Ca3Co4O9.
AB - (Graph Presented) Calcium cobaltite materials are synthesized by calcining the mixture of CaCO3 and Co3O4 with the Ca: Co ratio of 3:4. The reactivity of CaCO3 with Co3O4 is evaluated by thermogravimetric analysis (TGA), X-ray powder diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). Thermal expansion coefficient (TEC), electrical conductivity and electrochemical performance as intermediate-temperature solid oxide fuel cells (IT-SOFCs) cathode of as-prepared materials are characterized. The experiment results show that simultaneous decomposition of CaCO3 with calcium cobaltite formation occurs at 650-900°C. The average valence for Co ions of calcium cobaltite increases with temperature in the range of 750-900°C, involved in the formation of the compounds Ca3Co4O9 and Ca9Co12O28 at 800 and 900°C, respectively. The performance of calcium cobaltite cathodes applied in IT-SOFCs is significantly effected by the oxidation state of cobalt ions. As a result, Ca9Co12O28 cathode has a lower area specific resistance (e.g. 41.8% lower at 800°C) and higher peak power density (e.g. 45.0% higher at 800° C) than the cathode of Ca3Co4O9.
KW - Calcined temperature
KW - Calcium cobaltite cathode
KW - Electrochemical performance
KW - Solid oxide fuel cell
UR - http://www.scopus.com/inward/record.url?scp=84921748825&partnerID=8YFLogxK
U2 - 10.1016/j.jpowsour.2015.01.150
DO - 10.1016/j.jpowsour.2015.01.150
M3 - 文章
AN - SCOPUS:84921748825
SN - 0378-7753
VL - 280
SP - 581
EP - 587
JO - Journal of Power Sources
JF - Journal of Power Sources
ER -