N2 - To study the suppression of different porous materials on the explosion of combustible gas, some experiments were implemented. The porous materials were categorized into three kinds, including six subcategories, and the explosion suppression characteristics of the thin iron hoop, one-layer porous materials, two-layer composite porous materials, and three-layer composite porous materials were studied and analyzed. The results show that a rarefaction wave appears in the spherical vessel during the rapid development stage of combustion explosion. Further, the thin iron hoop could enhance the gas explosion intensity. And the explosion intensity suppression effect of the porous materials is obvious, the best effects of one-layer, two-layer and three-layer porous materials are from Fe–Ni 10 mm/40 PPI, Fe–Ni 10 mm/90 PPI + Al2O3 10 mm/30 PPI, and Al2O3 10 mm/50 PPI + Fe–Ni 10 mm/40 PPI + SiC 20 mm/20 PPI, respectively. According to the surface morphology of the porous materials, the anti-sintering ability of the three categories of porous materials follows the order of Al2O3 > SiC > Fe–Ni. Besides, the thickness and pore size of the combined porous material was changed, which has a great influence on the explosion pressure and the explosion intensity.
AB - To study the suppression of different porous materials on the explosion of combustible gas, some experiments were implemented. The porous materials were categorized into three kinds, including six subcategories, and the explosion suppression characteristics of the thin iron hoop, one-layer porous materials, two-layer composite porous materials, and three-layer composite porous materials were studied and analyzed. The results show that a rarefaction wave appears in the spherical vessel during the rapid development stage of combustion explosion. Further, the thin iron hoop could enhance the gas explosion intensity. And the explosion intensity suppression effect of the porous materials is obvious, the best effects of one-layer, two-layer and three-layer porous materials are from Fe–Ni 10 mm/40 PPI, Fe–Ni 10 mm/90 PPI + Al2O3 10 mm/30 PPI, and Al2O3 10 mm/50 PPI + Fe–Ni 10 mm/40 PPI + SiC 20 mm/20 PPI, respectively. According to the surface morphology of the porous materials, the anti-sintering ability of the three categories of porous materials follows the order of Al2O3 > SiC > Fe–Ni. Besides, the thickness and pore size of the combined porous material was changed, which has a great influence on the explosion pressure and the explosion intensity.
KW - Anti-sintering
KW - CH/Air mixture
KW - Explosion intensity
KW - Explosion suppression
KW - Porous material
UR - http://www.scopus.com/inward/record.url?scp=85082428158&partnerID=8YFLogxK
U2 - 10.1016/j.jlp.2020.104106
DO - 10.1016/j.jlp.2020.104106
M3 - 文章
AN - SCOPUS:85082428158
SN - 0950-4230
VL - 65
JO - Journal of Loss Prevention in the Process Industries
JF - Journal of Loss Prevention in the Process Industries
M1 - 104106
ER -