摘要
Foldable supercapacitors are desired for the next generation of wearable electronics. In this study, highly foldable graphene sponges with a honeycomb structure are prepared at 300 °C using the convenient thermal exfoliation process. A slow heating rate (5-10 °C·min-1) around 200 °C and an external confinement force are critical to a favorable exfoliation degree and uniform thickness of the graphene sponges. After being annealed at 1050 °C for 1 h, the conductivity of the graphene sponge has been improved from 2700 to 6900 S·m-1 without degrading its flexibility. The capacitance of the annealed graphene sponge has been measured in an aqueous electrolyte solution of 1 M Na2SO4. Its best capacitance is 138.74 F·g-1, and it reduces by 3.6% at a half-fold state and by 8.9% at a quarter-fold state.
源语言 | 英语 |
---|---|
页(从-至) | 2946-2952 |
页数 | 7 |
期刊 | Industrial and Engineering Chemistry Research |
卷 | 59 |
期 | 7 |
DOI | |
出版状态 | 已出版 - 19 2月 2020 |