T1 - Influence of Fe powders replacing Cu powders on the thermal and mechanical properties of aluminate cementitious thermal energy storage materials at high temperature
AU - Du, Aihong
AU - Yuan, Huiwen
AU - Liao, Wei
AU - Zhou, Haobo
AU - Lu, Chunhua
AU - Xu, Zhongzi
N1 - Publisher Copyright:
© 2016 Elsevier Ltd
PY - 2017/3/5
Y1 - 2017/3/5
N2 - Cost-effective thermal energy storage materials are vital to the application of solar thermal power plants. One focus of this paper is improving thermal and mechanical properties of the thermal energy storage materials; the second focus lies in reducing the investment cost. On the basis of aluminate cementitious composites with 1 wt% nano-SiO2, 1 wt% nano-Cu and 15 wt% Cu powders, we introduced different wt% (0, 5, 10, and 15) of Fe powders to gradually replace 15 wt% Cu powders. The samples were heated at 105, 350, and 900 °C, respectively. As a result, when the content of Fe powders substitution was 10 wt%, volume heat capacity, thermal conductivity and compressive strength of the composites after heat-treatment at 900 °C were up to 2.38 MJ m−3 K−1, 1.45 W m−1 K−1, and 73.8 MPa respectively, which were 26.6%, 26.1%, and 24.0% higher than those of the composites with 15 wt% Cu powders. At the same time, the investment of the composites with 10 wt% Fe powders substitution was reduced almost 62.0%, compared with that of the composites with 15 wt% Cu powders. In addition, XRD and MIP were employed to characteristic the mineral phases and the pore structures of the aluminate cementitious composites, respectively.
AB - Cost-effective thermal energy storage materials are vital to the application of solar thermal power plants. One focus of this paper is improving thermal and mechanical properties of the thermal energy storage materials; the second focus lies in reducing the investment cost. On the basis of aluminate cementitious composites with 1 wt% nano-SiO2, 1 wt% nano-Cu and 15 wt% Cu powders, we introduced different wt% (0, 5, 10, and 15) of Fe powders to gradually replace 15 wt% Cu powders. The samples were heated at 105, 350, and 900 °C, respectively. As a result, when the content of Fe powders substitution was 10 wt%, volume heat capacity, thermal conductivity and compressive strength of the composites after heat-treatment at 900 °C were up to 2.38 MJ m−3 K−1, 1.45 W m−1 K−1, and 73.8 MPa respectively, which were 26.6%, 26.1%, and 24.0% higher than those of the composites with 15 wt% Cu powders. At the same time, the investment of the composites with 10 wt% Fe powders substitution was reduced almost 62.0%, compared with that of the composites with 15 wt% Cu powders. In addition, XRD and MIP were employed to characteristic the mineral phases and the pore structures of the aluminate cementitious composites, respectively.
KW - Cementitious materials
KW - Cu powders
KW - Fe powders
KW - Properties
KW - Thermal energy storage
UR - http://www.scopus.com/inward/record.url?scp=85002194581&partnerID=8YFLogxK
U2 - 10.1016/j.applthermaleng.2016.11.139
DO - 10.1016/j.applthermaleng.2016.11.139
M3 - 文章
AN - SCOPUS:85002194581
SN - 1359-4311
VL - 114
SP - 148
EP - 153
JO - Applied Thermal Engineering
JF - Applied Thermal Engineering
ER -