Influence of oxidation to small punch creep test

Jianhua Shan, Zhenmei Qian, Xiang Ling

科研成果: 期刊稿件会议文章同行评审

5 引用 (Scopus)

摘要

In order to validate a procedure for creep rupture tests using small punch specimens, the influences of oxidation on the creep deflection curve, rupture time and ductility of miniature specimens were investigated. Using disc test specimens of 10mm in diameter and 0.5mm in thickness, a variety of small punch creep (SPC) tests for Cr5Mo steel at the condition of 550°C-404N and 650°C-189N under the protection of different Argon flow and in air atmosphere were firstly carried out. Metallographic observations, micro-hardness testing and measurement for these specimens of SPC test were performed. It indicates that the oxidized layer of specimens integrates and the residual thickness of specimens increases, while the hardness of specimens increases with the increment of the Argon flow. Moreover, the different oxidation degrees of specimens with the surface morphology were compared in this paper. The test results show the rupture time of specimens can be effectively prolonged by the protection of different Argon flow.

源语言英语
页(从-至)461-464
页数4
期刊Key Engineering Materials
353-358
PART 1
DOI
出版状态已出版 - 2007
活动Asian Pacific Conference for Fracture and Strength (APCFS'06) - Sanya, Hainan Island, 中国
期限: 22 11月 200625 11月 2006

指纹

探究 'Influence of oxidation to small punch creep test' 的科研主题。它们共同构成独一无二的指纹。

引用此