Plasma activation and atomic layer deposition of TiO2 on polypropylene membranes for improved performances of lithium-ion batteries

He Chen, Qian Lin, Qiang Xu, Yang Yang, Zongping Shao, Yong Wang

科研成果: 期刊稿件文章同行评审

134 引用 (Scopus)

摘要

Atomic layer deposition (ALD) of TiO2 was applied on porous polypropylene (PP) membranes which were used as separators in lithium-ion batteries (LIBs) composed of Li4Ti5O12 (LTO) anode/Li cathode. Without plasma activation on the bare PP membrane, the initial deposition of TiO2 was based on the subsurface nucleation mechanism, which prevented the formation of a conformal hydrophilic TiO2 layer at low ALD cycles. The improvement of wettability of the PP membrane to the electrolyte could only be achieved at high ALD cycles up to 500. However, the severe narrowing of membrane pores counterbalanced the wetting enhancement, which hardly improved the performance of the LIBs. Plasma pretreatment was efficient to generate active groups on the highly chemically inert surface of polypropylene membranes, thus ultrathin TiO2 films could be conformally deposited by ALD on the membrane surface based on the layer-by-layer mechanism at cycles as low as 20. Such a conformal ultrathin layer of TiO2 was confirmed to concurrently overcome both the thermal shrinkage and poor wettability of the PP membranes. Beneficial from the improved wettability at no expense of pore size, the electrochemical performances of LIBs such as specific discharge capacities at different discharge rates were upgraded.

源语言英语
页(从-至)217-224
页数8
期刊Journal of Membrane Science
458
DOI
出版状态已出版 - 15 5月 2014

指纹

探究 'Plasma activation and atomic layer deposition of TiO2 on polypropylene membranes for improved performances of lithium-ion batteries' 的科研主题。它们共同构成独一无二的指纹。

引用此