N2 - Hydriding combustion synthesis (HCS) has been regarded as an innovative process to produce magnesium based hydrogen storage alloys. In the present paper, a Mg-Mg2Ni composite hydrogen storage alloy was prepared by the HCS process under moderate conditions. Phase composition, synthesis mechanism and hydrogen storage properties were investigated by means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and pressure composition temperature (PCT). The results indicated that the HCS product was composed mainly of MgH2, Mg2NiH4 and Mg 2NiH0.3. A gas-solid reaction mechanism played an important role in the HCS process. The hydriding activity of the as synthesised product was very high so that it absorbed 4.61 mass% hydrogen in the first hydriding process without any activation treatment and the maximum hydrogen storage capacity achieved was 5.24 mass%. Moreover, the hydriding rate was excellent. For example, it could absorb >3.20 and 4.05 mass% hydrogen within 4 min in the first and forth hydriding/dehydriding cycle respectively. The relationships between the plateau pressure and temperature were: IgP(0.1 MPa)=-4250.5/T+7.9635 (hydriding), IgP(0.1 MPa)= -4125.4/T+ 7.6502 (dehydriding) for the lower plateau, and IgP(0.1 MPa)= -2894.6/T+ 5.9656 (hydriding), IgP(0.1 MPa)= -3855.9/T+ 7.3435 (dehydriding) for the higher plateau.
AB - Hydriding combustion synthesis (HCS) has been regarded as an innovative process to produce magnesium based hydrogen storage alloys. In the present paper, a Mg-Mg2Ni composite hydrogen storage alloy was prepared by the HCS process under moderate conditions. Phase composition, synthesis mechanism and hydrogen storage properties were investigated by means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and pressure composition temperature (PCT). The results indicated that the HCS product was composed mainly of MgH2, Mg2NiH4 and Mg 2NiH0.3. A gas-solid reaction mechanism played an important role in the HCS process. The hydriding activity of the as synthesised product was very high so that it absorbed 4.61 mass% hydrogen in the first hydriding process without any activation treatment and the maximum hydrogen storage capacity achieved was 5.24 mass%. Moreover, the hydriding rate was excellent. For example, it could absorb >3.20 and 4.05 mass% hydrogen within 4 min in the first and forth hydriding/dehydriding cycle respectively. The relationships between the plateau pressure and temperature were: IgP(0.1 MPa)=-4250.5/T+7.9635 (hydriding), IgP(0.1 MPa)= -4125.4/T+ 7.6502 (dehydriding) for the lower plateau, and IgP(0.1 MPa)= -2894.6/T+ 5.9656 (hydriding), IgP(0.1 MPa)= -3855.9/T+ 7.3435 (dehydriding) for the higher plateau.
KW - Hydriding combustion synthesis
KW - Hydrogen storage property
KW - Magnesium based hydrogen storage alloy
KW - Synthesis mechanism
UR - http://www.scopus.com/inward/record.url?scp=55749105108&partnerID=8YFLogxK
U2 - 10.1179/174328407X161358
DO - 10.1179/174328407X161358
M3 - 文章
AN - SCOPUS:55749105108
SN - 0267-0836
VL - 24
SP - 1309
EP - 1312
JO - Materials Science and Technology (United Kingdom)
JF - Materials Science and Technology (United Kingdom)
IS - 11
ER -