W-type barium hexaferrites doped with Sm3+, Ba1-xSmxCo2Fe16O27 (x = 0.0, 0.05, 0.1, 0.15, 0.2) were prepared by the conventional solid-state reaction. The structure and electromagnetic properties of the calcined samples were studied using powder X-ray diffraction (XRD) and network analyzer (Agilent 8722ET). All the XRD patterns showed the single phase of the magnetoplumbite barium ferrite without other intermediate phase when x ≤ 0.15. The microwave electromagnetic properties of the samples have been studied at the frequency range from 2 GHz to 18 GHz. It was shown that ε′ and ε″ increased slightly, and the maximum of ε″ shifted to low frequency position with Sm3+ ions doping. The μ″ and μ′ values were improved significantly when x = 0.15, and the peak value of μ″ was about 1.6 at 7 GHz and 1.75 at 18 GHz position, respectively, exhibiting excellent microwave magnetic performance. Furthermore, the reasons have also been discussed using electromagnetic theory. Ba0.85Sm0.15Co2Fe16O27 powders (85% by weight) were mixed with epoxy resin to form compound coating materials with different thicknesses, the reflection loss values of which were also measured. It is shown that the reflection loss value increases with the increase of the coating thickness under our experimental range. The maximum of reflection loss reached about -23 dB and it was below -10 dB at the frequency range from 8 GHz to 18 GHz, when the thickness was 1.8 mm.

源语言英语
页(从-至)863-866
页数4
期刊Journal of Alloys and Compounds
481
1-2
DOI
出版状态已出版 - 29 7月 2009

指纹

探究 'The microwave magnetic performance of Sm3+ doped BaCo2Fe16O27' 的科研主题。它们共同构成独一无二的指纹。

引用此