T1 - Versatile Bioactive Glass/Zeolitic Imidazolate Framework-8-Based Skin Scaffolds toward High-Performance Wound Healing
AU - Hou, Yongchun
AU - Xu, Xiaowei
AU - Zhou, Yaqin
AU - Li, Qing
AU - Zhu, Liangliang
AU - Liu, Chang
AU - Chen, Su
AU - Pang, Jie
N1 - Publisher Copyright:
© 2024 American Chemical Society.
PY - 2024/2/21
Y1 - 2024/2/21
N2 - Designing a novel biomaterial for wound healing is based on biocompatibility and excellent mechanical strength. In this study, bioactive glass (BG) and zeolitic imidazolate framework-8 (ZIF-8) have been incorporated into poly(ϵ-caprolactone)/poly(vinyl alcohol) (PCL/PVA) composite skin scaffolds via microfluidic electrospinning. Interestingly, the addition of ZIF-8 further strengthens the BG stability and demonstrates better antibacterial effects. Utilizing the slow release of Zn, Ca, and Si ions, it also significantly promotes growth factor expression and skin regeneration. In addition, it is further demonstrated by in vitro and in vivo studies that the prepared composite skin scaffolds possess excellent biocompatibility, antibacterial capabilities, and mechanical properties. The prepared BG/ZIF-8-loaded scaffold possesses high tensile strength (26 MPa) and excellent antibacterial properties (achieves 89.64 and 78.8% inhibition of E. coli and S. aureus, respectively), and cell viability increased by 51.2%. More importantly, the wound shrinkage of the BG/ZIF-8-loaded scaffold is better than that of an unloaded scaffold, and the shrinkage rates of PCL/PVA@BG/ZIF-8(1 wt %) group is 95% with 2.2 mm granulation growth thickness within 12 days. Thus, the composite skin scaffold loaded with BG/ZIF-8 prepared by microfluidic electrospinning provides a new perspective for accelerating wound healing and is a potential novel therapeutic strategy for efficient wound healing.
AB - Designing a novel biomaterial for wound healing is based on biocompatibility and excellent mechanical strength. In this study, bioactive glass (BG) and zeolitic imidazolate framework-8 (ZIF-8) have been incorporated into poly(ϵ-caprolactone)/poly(vinyl alcohol) (PCL/PVA) composite skin scaffolds via microfluidic electrospinning. Interestingly, the addition of ZIF-8 further strengthens the BG stability and demonstrates better antibacterial effects. Utilizing the slow release of Zn, Ca, and Si ions, it also significantly promotes growth factor expression and skin regeneration. In addition, it is further demonstrated by in vitro and in vivo studies that the prepared composite skin scaffolds possess excellent biocompatibility, antibacterial capabilities, and mechanical properties. The prepared BG/ZIF-8-loaded scaffold possesses high tensile strength (26 MPa) and excellent antibacterial properties (achieves 89.64 and 78.8% inhibition of E. coli and S. aureus, respectively), and cell viability increased by 51.2%. More importantly, the wound shrinkage of the BG/ZIF-8-loaded scaffold is better than that of an unloaded scaffold, and the shrinkage rates of PCL/PVA@BG/ZIF-8(1 wt %) group is 95% with 2.2 mm granulation growth thickness within 12 days. Thus, the composite skin scaffold loaded with BG/ZIF-8 prepared by microfluidic electrospinning provides a new perspective for accelerating wound healing and is a potential novel therapeutic strategy for efficient wound healing.
KW - bioactive glass
KW - fiber scaffolds
KW - microfluidic electrospinning
KW - wound healing
KW - zeolitic imidazolate framework-8
UR - http://www.scopus.com/inward/record.url?scp=85185339097&partnerID=8YFLogxK
U2 - 10.1021/acsami.3c14529
DO - 10.1021/acsami.3c14529
M3 - 文章
C2 - 38343190
AN - SCOPUS:85185339097
SN - 1944-8244
VL - 16
SP - 8228
EP - 8237
JO - ACS Applied Materials and Interfaces
JF - ACS Applied Materials and Interfaces
IS - 7
ER -