Warm pre-strain: Strengthening the metastable 304L austenitic stainless steel without compromising its hydrogen embrittlement resistance

Yanfei Wang, Zhiling Zhou, Weijie Wu, Jianming Gong

科研成果: 期刊稿件文章同行评审

5 引用 (Scopus)

摘要

Plastic pre-strains were applied to the metastable 304L austenitic stainless steel at both room temperature (20 °C) and higher temperatures (i.e., 50, 80 and 100 °C), and then the hydrogen embrittlement (HE) susceptibility of the steel was evaluated by cathodically hydrogen-charging and tensile testing. The 20 °C pre-strain greatly strengthened the steel, but simultaneously significantly increased the HE susceptibility of the steel, since α' martensite was induced by the pre-strain, causing the pre-existence of α' martensite, which provided "highways" for hydrogen to transport deep into the steel during the hydrogen-charging. Although the warm pre-strains did not strengthen the steel as significantly as the 20 °C pre-strain, they retained the HE resistance of the steel. This is because the higher temperatures, particularly 80 and 100 °C, suppressed the α' martensite transformation during the pre-straining. Pre-strain at a temperature slightly higher than room temperature has a potential to strengthen the metastable 304L austenitic stainless steel without compromising its initial HE resistance.

源语言英语
文章编号1331
期刊Materials
10
11
DOI
出版状态已出版 - 21 11月 2017

指纹

探究 'Warm pre-strain: Strengthening the metastable 304L austenitic stainless steel without compromising its hydrogen embrittlement resistance' 的科研主题。它们共同构成独一无二的指纹。

引用此