Atomic layer deposition of alumina on porous polytetrafluoroethylene membranes for enhanced hydrophilicity and separation performances

Qiang Xu, Yang Yang, Xiaozu Wang, Zhaohui Wang, Wanqin Jin, Jun Huang, Yong Wang

Research output: Contribution to journalArticlepeer-review

98 Scopus citations

Fingerprint

Dive into the research topics of 'Atomic layer deposition of alumina on porous polytetrafluoroethylene membranes for enhanced hydrophilicity and separation performances'. Together they form a unique fingerprint.

Chemical Engineering