Inhibitory effect of konjac glucomanan on pitting corrosion of AA5052 aluminium alloy in NaCl solution

Kegui Zhang, Wenzhong Yang, Bin Xu, Yun Chen, Xiaoshuang Yin, Ying Liu, Huanzhen Zuo

Research output: Contribution to journalArticlepeer-review

104 Scopus citations

Fingerprint

Dive into the research topics of 'Inhibitory effect of konjac glucomanan on pitting corrosion of AA5052 aluminium alloy in NaCl solution'. Together they form a unique fingerprint.

Material Science