Investigation of the internal physical and chemical changes of a cylindrical lithium-ion battery during thermal runaway

Tengfei He, Siddharth Gadkari, Teng Zhang, Zhirong Wang, Jialong Liu, Ning Mao, Jinglong Bai, Qiong Cai

Research output: Contribution to journalArticlepeer-review

10 Scopus citations

Abstract

This study delves into the critical safety issue of thermal runaway (TR) in lithium-ion batteries (LIBs), particularly focusing on the physical and chemical changes occurring in the electrode materials during temperature escalation. We investigate a commercial 18650 type 2.6 Ah Li[Ni5Co2Mn3]O2/graphite battery, tracing changes from room temperature to the point of TR. Our findings reveal that the negative electrode experiences gradual decomposition and regeneration of the solid electrolyte interface (SEI) film, reacting with the electrolyte to form compounds such as Li2CO3 and LiF on its surface. Similarly, the positive electrode also generates Li2CO3 on its surface as temperature rises. Notably, at 185 °C, there is a partial disintegration of the positive electrode particles, accompanied by a structural transformation from the LiMO2 (M representing Ni, Co, and Mn) R-3m layered structure to a disordered spinel LiM2O4. This research contributes to a deeper understanding of the TR mechanism in LIBs, offering valuable insights for material researchers in designing safer battery systems.

Original languageEnglish
Article number140548
JournalJournal of Cleaner Production
Volume434
DOIs
StatePublished - 1 Jan 2024

Keywords

  • Decomposition reaction
  • Lithium-ion battery
  • Particles broken
  • Phase change
  • Thermal runaway mechanism