Stress Corrosion Cracking of Ultrafine-Grained Ti-2Fe-0.1B Alloying after Equal Channel Angular Pressing

Shuai Huang, Yutong Jin, Yu Wang, Yuecheng Dong, Hui Chang, Igor V. Alexandrov

Research output: Contribution to journalArticlepeer-review

5 Scopus citations

Fingerprint

Dive into the research topics of 'Stress Corrosion Cracking of Ultrafine-Grained Ti-2Fe-0.1B Alloying after Equal Channel Angular Pressing'. Together they form a unique fingerprint.

Material Science