Abstract
The MgAPO-36 molecular sieve films on porous α-Al2O 3 substrates were synthesized under different nmg/np ratios by using in situ hydrothermal crystallization. The influence of n mg/np on the microstructure and continuity of the MgAPO-36 film was studied. The CoAPO-36 molecular sieve films on porous α-Al 2O3, stainless steel and K2Ti6O 13 substrates were fabricated to reveal the effect of the substrate on film formation. SEM observations and XRD data indicate that the pure MgAPO-36 film can be fabricated on porous α-Al2O3 substrate with the nmg/np ratio between 0.08 and 0.24. Especially, the MgAPO-36 film becomes uniform and continuous when the nmg/np ratio is about 0.10. Although pure CoAPO-36 films can be formed on porous α-Al 2O3, stainless steel and K2Ti6O 13 substrates, the continuous and uniform CoAPO-36 film can only be synthesized on porous K2Ti6O13substrate.
Original language | English |
---|---|
Pages (from-to) | 1307-1310 |
Number of pages | 4 |
Journal | Chinese Journal of Inorganic Chemistry |
Volume | 26 |
Issue number | 7 |
State | Published - Jul 2010 |
Keywords
- Aluminophosphate molecular sieve film
- CoAPO-36
- MgAPO-36