Atomic-layer-deposition-enabled nonwoven membranes with hierarchical ZnO nanostructures for switchable water/oil separations

Sen Xiong, Liang Kong, Jun Huang, Xiaoqiang Chen, Yong Wang

科研成果: 期刊稿件文章同行评审

69 引用 (Scopus)

指纹

探究 'Atomic-layer-deposition-enabled nonwoven membranes with hierarchical ZnO nanostructures for switchable water/oil separations' 的科研主题。它们共同构成独一无二的指纹。

Engineering

Material Science