Atomic Layer Deposition of a Pt-Skin Catalyst for Base-Free Aerobic Oxidation of 5-Hydroxymethylfurfural to 2,5-Furandicarboxylic Acid
Jinshan Shen, Hao Chen, Kequan Chen, Yong Qin, Xiuyang Lu, Pingkai Ouyang, Jie Fu
科研成果: 期刊稿件 › 文章 › 同行评审