Atomic layer deposition of TiO2 on carbon-nanotubes membrane for capacitive deionization removal of chromium from water

Jianhua Feng, Sen Xiong, Li Ren, Yong Wang

科研成果: 期刊稿件文章同行评审

31 引用 (Scopus)

指纹

探究 'Atomic layer deposition of TiO2 on carbon-nanotubes membrane for capacitive deionization removal of chromium from water' 的科研主题。它们共同构成独一无二的指纹。

Chemical Engineering

Material Science