摘要
Cold sintering has attracted significant attention as its remarkably rapid densification process at low sintering temperatures leads to considerable energy savings. However, the sintering behaviors of cold-sintered perovskite ceramics remain poorly understood and lack precise control over material microstructure. Here, we fabricated dense SrCo0.8Fe0.2O3−δ (SCF) ceramic oxygen permeation membranes by cold sintering. Adding an appropriate ratio of sub-micron SCF particles can better bridge the sintering interspaces between micron particles, generate amorphous phase through “dissolution-precipitation,” and aid in the initial densification. The average relative density of SCF membranes undergoes a significant increase to 95.9% after cold sintering and post-annealing at 900°C, which is much lower than the temperature required for conventional high-temperature solid-state sintering (>1200°C). The oxygen permeation flux of the prepared SCF perovskite membrane reaches 2.8 mL min−1 cm−2, which proves that this method has the potential to be an excellent sintering technique for dense perovskite ceramic membranes.
源语言 | 英语 |
---|---|
文章编号 | e18378 |
期刊 | AIChE Journal |
卷 | 70 |
期 | 4 |
DOI | |
出版状态 | 已出版 - 4月 2024 |