TY - JOUR
T1 - Preparation of absorptive material containing comb-like flexible quaternary amm onium chain
AU - Lei, Wen
AU - Wei, Rongqing
AU - Liu, Xiaoning
AU - Ding, Lingpeng
AU - Wu, Hao
AU - Jiang, Min
PY - 2013/6
Y1 - 2013/6
N2 - A strong base anion exchange resin with comb-like flexible chain(flex-AIQ-R)structure was synthesized by the reaction of triethylamine hydrochloride with comb-like epoxy resin which was prepared by atom transfer radical polymerization (ATRP), using the chloroacetyl styrene-divinylbenzene copolymer microspheres (PS-acyl-Cl) as the initiator and glycidyl methacrylate (GMA) as monomer. Several factors were discussed and optimized during the reaction, such as pH of the solution, reaction time, reaction temperature, the amount of catalyst and reagents. The final optimum conditions obtained are as follows: the pH value of the solution is 8~9, the reaction time is 10 h, reaction temperature is 90°C, catalyst amount is 2%, molar ratio of triethylamine hydrochloride and resin is 5:1, the amount of solvent is 10 mL/g and ethanol content is 40%. Under the above conditions, the conversion rate and maximum loading of the diethyl-amine can be up to 85% and 2.78 mmol/g, respectively.
AB - A strong base anion exchange resin with comb-like flexible chain(flex-AIQ-R)structure was synthesized by the reaction of triethylamine hydrochloride with comb-like epoxy resin which was prepared by atom transfer radical polymerization (ATRP), using the chloroacetyl styrene-divinylbenzene copolymer microspheres (PS-acyl-Cl) as the initiator and glycidyl methacrylate (GMA) as monomer. Several factors were discussed and optimized during the reaction, such as pH of the solution, reaction time, reaction temperature, the amount of catalyst and reagents. The final optimum conditions obtained are as follows: the pH value of the solution is 8~9, the reaction time is 10 h, reaction temperature is 90°C, catalyst amount is 2%, molar ratio of triethylamine hydrochloride and resin is 5:1, the amount of solvent is 10 mL/g and ethanol content is 40%. Under the above conditions, the conversion rate and maximum loading of the diethyl-amine can be up to 85% and 2.78 mmol/g, respectively.
KW - Anion exc hange resin
KW - Chloroacetyl poly(styrene-divinylbenzene)
KW - Comb-l ike flexible chain
KW - Epoxy resin
KW - Quaternary ammonium
KW - Strong basicity
UR - http://www.scopus.com/inward/record.url?scp=84880022399&partnerID=8YFLogxK
M3 - 文章
AN - SCOPUS:84880022399
SN - 1000-7555
VL - 29
SP - 24
EP - 27
JO - Gaofenzi Cailiao Kexue Yu Gongcheng/Polymeric Materials Science and Engineering
JF - Gaofenzi Cailiao Kexue Yu Gongcheng/Polymeric Materials Science and Engineering
IS - 6
ER -